11 Alloys Found

Alloy UNS#DesignationActiveView

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C17300

Beryllium Copper Yes C17300 Profile
Suppliers of C17300

C17400 *

Beryllium Copper No C17400 Profile
Suppliers of C17400

C17410 *

Beryllium Copper Yes C17410 Profile
Suppliers of C17410

C17460 *

Beryllium Copper Yes C17460 Profile
Suppliers of C17460

C17465

Beryllium Copper Yes C17465 Profile
Suppliers of C17465

C17530 *

Beryllium Copper Yes C17530 Profile
Suppliers of C17530

C82500 *

Beryllium Copper 20C Yes C82500 Profile
Suppliers of C82500

C82700 *

High Copper Alloy Yes C82700 Profile
Suppliers of C82700

C82800 *

Beryllium Copper 275C Yes C82800 Profile
Suppliers of C82800