25 Alloys Found

Alloy UNS#DesignationActiveView

C12500 *

Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile
Suppliers of C12500

C12700 *

Copper Alloy No C12700 Profile
Suppliers of C12700

C12800 *

Copper Alloy No C12800 Profile
Suppliers of C12800

C12900 *

Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile
Suppliers of C12900

C13000

Copper Alloy No C13000 Profile
Suppliers of C13000

C14300 *

Cadmium Copper, Deoxidized Yes C14300 Profile
Suppliers of C14300

C14310 *

Cadmium Copper No C14310 Profile
Suppliers of C14310

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C18661 *

Yes C18661 Profile
Suppliers of C18661

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C40800 *

Silicon Brass No C40800 Profile
Suppliers of C40800

C40810 *

Yes C40810 Profile
Suppliers of C40810

C40850 *

Yes C40850 Profile
Suppliers of C40850

C40860 *

Yes C40860 Profile
Suppliers of C40860

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C42200 *

Yes C42200 Profile
Suppliers of C42200

C42520 *

Yes C42520 Profile
Suppliers of C42520

C50780 *

Yes C50780 Profile
Suppliers of C50780

C51900 *

Yes C51900 Profile
Suppliers of C51900

C65400

Yes C65400 Profile
Suppliers of C65400

C66700 *

Manganese Brass Yes C66700 Profile
Suppliers of C66700

C76200

Nickel Silver Yes C76200 Profile
Suppliers of C76200
* signifies an alloy registered with the U.S. EPA as Antimicrobial.