46 Alloys Found

Alloy UNS#DesignationActiveView

C16200 *

Cadmium Copper Yes C16200 Profile
Suppliers of C16200

C16210 *

High Copper Alloy No C16210 Profile
Suppliers of C16210

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C18100

Yes C18100 Profile
Suppliers of C18100

C18160

Yes C18160 Profile
Suppliers of C18160

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19500 *

Yes C19500 Profile
Suppliers of C19500

C19800 *

Yes C19800 Profile
Suppliers of C19800

C19810 *

Hig Copper Alloy Yes C19810 Profile
Suppliers of C19810

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40800 *

Silicon Brass No C40800 Profile
Suppliers of C40800

C40820 *

Yes C40820 Profile
Suppliers of C40820

C40850 *

Yes C40850 Profile
Suppliers of C40850

C40860 *

Yes C40860 Profile
Suppliers of C40860

C40950 *

Yes C40950 Profile
Suppliers of C40950

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41120 *

Yes C41120 Profile
Suppliers of C41120

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C42500 *

Yes C42500 Profile
Suppliers of C42500

C42520 *

Yes C42520 Profile
Suppliers of C42520

C44710

Yes C44710 Profile
Suppliers of C44710

C50580 *

Yes C50580 Profile
Suppliers of C50580

C50590 *

Yes C50590 Profile
Suppliers of C50590

C50705 *

Yes C50705 Profile
Suppliers of C50705

C50780 *

Yes C50780 Profile
Suppliers of C50780

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51080 *

Yes C51080 Profile
Suppliers of C51080

C51100 *

Yes C51100 Profile
Suppliers of C51100

C51180 *

Yes C51180 Profile
Suppliers of C51180

C51900 *

Yes C51900 Profile
Suppliers of C51900

C51980 *

Yes C51980 Profile
Suppliers of C51980

C52100 *

Phospher Bronze, 8% C Yes C52100 Profile
Suppliers of C52100

C52180 *

Yes C52180 Profile
Suppliers of C52180

C52480 *

Yes C52480 Profile
Suppliers of C52480

C64725 *

Copper Silicon Alloy Yes C64725 Profile
Suppliers of C64725

C64780 *

Yes C64780 Profile
Suppliers of C64780

C66430 *

Yes C66430 Profile
Suppliers of C66430

C69240

Yes C69240 Profile
Suppliers of C69240

C69300 *

ECO Brass Yes C69300 Profile
Suppliers of C69300

C70260 *

Yes C70260 Profile
Suppliers of C70260

C70265 *

Yes C70265 Profile
Suppliers of C70265

C70280 *

Yes C70280 Profile
Suppliers of C70280

C72500 *

Yes C72500 Profile
Suppliers of C72500

C94700 *

Cast Nickel-Tin Bronze Yes C94700 Profile
Suppliers of C94700

C95500 *

Yes C95500 Profile
Suppliers of C95500
* signifies an alloy registered with the U.S. EPA as Antimicrobial.