7 Alloys Found

Alloy UNS#DesignationActiveView

C35000

Medium Leaded Brass, 62% Yes C35000 Profile
Suppliers of C35000

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C49300 *

Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile
Suppliers of C49300

C67420

Yes C67420 Profile
Suppliers of C67420

C69240

Yes C69240 Profile
Suppliers of C69240

C86300

Manganese Bronze Yes C86300 Profile
Suppliers of C86300

C94700 *

Cast Nickel-Tin Bronze Yes C94700 Profile
Suppliers of C94700
* signifies an alloy registered with the U.S. EPA as Antimicrobial.