3 Alloys Found

Alloy UNS#DesignationActiveView

C81800 *

Beryllium Copper 50C No C81800 Profile
Suppliers of C81800

C82000 *

Beryllium Copper 10C Yes C82000 Profile
Suppliers of C82000

C82200 *

Beryllium Copper 30C Yes C82200 Profile
Suppliers of C82200
* signifies an alloy registered with the U.S. EPA as Antimicrobial.