39 Alloys Found

Alloy UNS#DesignationActiveView

C15500 *

Yes C15500 Profile
Suppliers of C15500

C16500 *

Yes C16500 Profile
Suppliers of C16500

C17200 *

Beryllium Copper Yes C17200 Profile
Suppliers of C17200

C17300

Beryllium Copper Yes C17300 Profile
Suppliers of C17300

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17510 *

Beryllium Copper Yes C17510 Profile
Suppliers of C17510

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19200 *

Yes C19200 Profile
Suppliers of C19200

C19210 *

Yes C19210 Profile
Suppliers of C19210

C19400 *

Yes C19400 Profile
Suppliers of C19400

C35600

Extra High Leaded Brass Yes C35600 Profile
Suppliers of C35600

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40810 *

Yes C40810 Profile
Suppliers of C40810

C40850 *

Yes C40850 Profile
Suppliers of C40850

C40860 *

Yes C40860 Profile
Suppliers of C40860

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41120 *

Yes C41120 Profile
Suppliers of C41120

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C41900

Tin Brass No C41900 Profile
Suppliers of C41900

C42200 *

Yes C42200 Profile
Suppliers of C42200

C42500 *

Yes C42500 Profile
Suppliers of C42500

C44710

Yes C44710 Profile
Suppliers of C44710

C50580 *

Yes C50580 Profile
Suppliers of C50580

C50780 *

Yes C50780 Profile
Suppliers of C50780

C51000 *

Phosphor Bronze, 5% A Yes C51000 Profile
Suppliers of C51000

C51100 *

Yes C51100 Profile
Suppliers of C51100

C51180 *

Yes C51180 Profile
Suppliers of C51180

C51900 *

Yes C51900 Profile
Suppliers of C51900

C61500 *

Yes C61500 Profile
Suppliers of C61500

C66700 *

Manganese Brass Yes C66700 Profile
Suppliers of C66700

C69150 *

Copper Zinc Alloy (Copper Zinc Alloy) Yes C69150 Profile
Suppliers of C69150

C70600 *

Copper-Nickel, 10% Yes C70600 Profile
Suppliers of C70600

C71000 *

Copper-Nickel, 20% Yes C71000 Profile
Suppliers of C71000

C72500 *

Yes C72500 Profile
Suppliers of C72500

C73500 *

Nickel Silver Yes C73500 Profile
Suppliers of C73500

C76200

Nickel Silver Yes C76200 Profile
Suppliers of C76200

C81800 *

Beryllium Copper 50C No C81800 Profile
Suppliers of C81800

C82000 *

Beryllium Copper 10C Yes C82000 Profile
Suppliers of C82000

C82200 *

Beryllium Copper 30C Yes C82200 Profile
Suppliers of C82200
* signifies an alloy registered with the U.S. EPA as Antimicrobial.