10 Alloys Found

Alloy UNS#DesignationActiveView

C42210 *

Tin Brass Yes C42210 Profile
Suppliers of C42210

C49255

Copper-Zinc-Bismuth Yes C49255 Profile
Suppliers of C49255

C49300 *

Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile
Suppliers of C49300

C85690

Yes C85690 Profile
Suppliers of C85690

C89510 *

SeBiLOY I (EnviroBrass I) Yes C89510 Profile
Suppliers of C89510

C89520 *

SeBiLOY II (EnviroBrass II) Yes C89520 Profile
Suppliers of C89520

C89530

Copper-Bismuth-Selenium Alloy (Brasses) Yes C89530 Profile
Suppliers of C89530

C89535

Copper-Bismuth Alloy Yes C89535 Profile
Suppliers of C89535

C89540

Yes C89540 Profile
Suppliers of C89540

C89550 *

SeBiLOY III (EnviroBrass III) Yes C89550 Profile
Suppliers of C89550
* signifies an alloy registered with the U.S. EPA as Antimicrobial.