C28000 Bar
Supplier Type: Service Center
3000 Shermer RdNorthbrook, Illinois 60062-7713
United States(800) 999-2497
C28000 Billets
C28000 Castings
C28000 Extrusions
C28000 Fitting
C28000 Foil
C28000 Forgings
C28000 Ingot
C28000 Pipe
C28000 Plate
Supplier Type: Service Center
86 Tube DrReading, Pennsylvania 19605-9274
United States(800) 523-8263
Website: Cambridge-Lee Industries LLC
Supplier Type: Service Center
1340 Soldiers Field RdBoston, Massachusetts 02135-1000
United States
Website: Cambridge-Lee Industries LLC
Supplier Type: Service Center
1908 Strand StGalveston, Texas 77550-1629
United States(409) 765-6361
Website: Farmers Alloy Fabricating
Supplier Type: Service Center
9900 Emmett F Lowry ExpyTexas City, Texas 77591-2124
United States(409) 944-3000
Website: Farmers Copper Ltd.
Email: brent.farmer@wieland.com
Supplier Type: Fabricator
1000 Jorie Blvd Ste 111Oak Brook, Illinois 60523-4484
United States(630) 990-2025
Website: KME America
Email: sales@kmeamerica.com
Supplier Type: Fabricator
5300 Willow Creek Dr SWCedar Rapids, Iowa 52404-4303
United States(319) 368-7700
Website: PMX Industries, Inc.
Supplier Type: Service Center
350 S Grand Ave Ste 5100Los Angeles, California 90071-3421
United States(213) 687-7700
Website: Reliance Steel and Aluminum Co.
Email: dsargent@rsac.com
C28000 Rod
Supplier Type: Service Center
3000 Shermer RdNorthbrook, Illinois 60062-7713
United States(800) 999-2497
C28000 Shapes
C28000 Sheet
Supplier Type: Service Center
86 Tube DrReading, Pennsylvania 19605-9274
United States(800) 523-8263
Website: Cambridge-Lee Industries LLC
Supplier Type: Service Center
1340 Soldiers Field RdBoston, Massachusetts 02135-1000
United States
Website: Cambridge-Lee Industries LLC
Supplier Type: Service Center
1908 Strand StGalveston, Texas 77550-1629
United States(409) 765-6361
Website: Farmers Alloy Fabricating
Supplier Type: Service Center
9900 Emmett F Lowry ExpyTexas City, Texas 77591-2124
United States(409) 944-3000
Website: Farmers Copper Ltd.
Email: brent.farmer@wieland.com
Supplier Type: Service Center
6960 79th StMiddle Village, New York 11379-2933
United States(800) 221-5579
Website: Lewis Brass & Copper Company
Email: sales@lewisbrass.com
Supplier Type: Service Center
2950 Turnpike DrHatboro, Pennsylvania 19040-4200
United States(215) 675-4645
Website: Marmetal Industries, LLC
Email: sales@marmetal.com
Supplier Type: Service Center
3000 Shermer RdNorthbrook, Illinois 60062-7713
United States(800) 999-2497
Supplier Type: Service Center
5775 Monaco StCommerce City, Colorado 80022-4064
United States(303) 286-9700
Website: Olympic Metals, Inc.
Email: ggibb@rsac.com
Supplier Type: Fabricator
5300 Willow Creek Dr SWCedar Rapids, Iowa 52404-4303
United States(319) 368-7700
Website: PMX Industries, Inc.
Supplier Type: Service Center
35 Indel AveRancocas, New Jersey 08073
United States(609) 267-4120
Website: Rancocas Metals Corp.
Email: Sales@rancocasmetals.com
Supplier Type: Service Center
350 S Grand Ave Ste 5100Los Angeles, California 90071-3421
United States(213) 687-7700
Website: Reliance Steel and Aluminum Co.
Email: dsargent@rsac.com
Supplier Type: Service Center
2621 W 15th PlChicago, Illinois 60608-1712
United States(773) 762-2121
Website: Ryerson
Email: keith.kessler@ryerson.com
Supplier Type: Service Center
2289 Industrial Pkwy WHayward, California 94545-5026
United States(510) 887-5525
Website: Sequoia Brass & Copper
Email: sales@sequoia-brass-copper.com
Supplier Type: Service Center
1401 Brook DrDowners Grove, Illinois 60515-1077
United States(630) 629-9340
Website: United States Brass & Copper
Email: sales@usbrassandcopper.com
Supplier Type: Fabricator
70 Sayre StBuffalo, New York 14207-2225
United States(716) 879-6700
Website: Wieland Rolled Products NA
Supplier Type: Service Center
125 Strafford Ave Ste 108Wayne, Pennsylvania 19087-3335
United States(877) 499-1544
Website: Williams Metals and Welding Alloys, Inc.
Email: sales@wmwa.net
C28000 Slab
C28000 Strip
Supplier Type: Service Center
1340 Soldiers Field RdBoston, Massachusetts 02135-1000
United States
Website: Cambridge-Lee Industries LLC
Supplier Type: Service Center
6960 79th StMiddle Village, New York 11379-2933
United States(800) 221-5579
Website: Lewis Brass & Copper Company
Email: sales@lewisbrass.com
Supplier Type: Fabricator
5300 Willow Creek Dr SWCedar Rapids, Iowa 52404-4303
United States(319) 368-7700
Website: PMX Industries, Inc.
Supplier Type: Fabricator
1637 Elmwood AveCranston, Rhode Island 02910-4937
United States(401) 434-7640
Website: Scott Brass Inc.
Supplier Type: Fabricator
70 Sayre StBuffalo, New York 14207-2225
United States(716) 879-6700
Website: Wieland Rolled Products NA
C28000 Tube
Supplier Type: Service Center
2289 Industrial Pkwy WHayward, California 94545-5026
United States(510) 887-5525
Website: Sequoia Brass & Copper
Email: sales@sequoia-brass-copper.com
C28000 Wire
Please note: Alloys marked with * are registered with the U.S. EPA as Antimicrobial