Loading...
C87610 Bar
C87610 Billets
C87610 Castings
C87610 Extrusions
C87610 Fitting
C87610 Foil
C87610 Forgings
C87610 Ingot
The Federal Metal CompanyA member of the CDA
Bedford, Ohio 44146-5406
United States(440) 232-8700
Website: The Federal Metal Company
Supplier Type: Fabricator
7250 Division StBedford, Ohio 44146-5406
United States(440) 232-8700
Website: The Federal Metal Company
C87610 Pipe
C87610 Plate
C87610 Rod
C87610 Shapes
C87610 Sheet
C87610 Slab
C87610 Strip
C87610 Tube
C87610 Wire
Please note: Alloys marked with * are registered with the U.S. EPA as Antimicrobial