A Copper Alliance Member

Copper Alloys Advanced Search

Loading...

C33000 Bar

C33000 Billets

C33000 Castings

C33000 Extrusions

C33000 Fitting

C33000 Foil

C33000 Forgings

C33000 Ingot

C33000 Pipe

C33000 Plate

C33000 Rod

C33000 Shapes

C33000 Sheet

C33000 Slab

C33000 Strip

C33000 Tube

Cambridge-Lee Industries LLC

Supplier Type: Service Center

1340 Soldiers Field Rd
Boston, MA 02135-1000
UNITED STATES
(800) 352-9052
(617) 787-7823
Website: Cambridge-Lee Industries LLC
Copper and Brass Sales, Inc

Supplier Type: Service Center

22355 West Eleven Mile Road
Southfield, MI 48033
UNITED STATES
(248) 233-5703
(317) 852-1726
Website: Copper and Brass Sales, Inc
Drawn Metal Tube Co.A member of the CDA

Supplier Type: Fabricator

219 Elm St
Thomaston, CT 06787-1709
UNITED STATES
(860) 283-4345
(860) 283-8233
Website: Drawn Metal Tube Co.
Farmers Alloy Fabricating

Supplier Type: Service Center

1908 Strand Street
Galveston, TX 77550
UNITED STATES
(409) 765-6361
(409) 765-7115
Website: Farmers Alloy Fabricating
Farmers Copper Ltd.

Supplier Type: Service Center

9900 Emmett F Lowry Expy
Texas City, TX 77591
UNITED STATES
(409) 944-3000
Website: Farmers Copper Ltd.
Email:
H&H Tube and Manufacturing Co.

Supplier Type: Fabricator

PO BOX 455
108 Garfield Street
Vanderbilt, MI 49795-0455
UNITED STATES
(989) 983-2800
(989) 983-4530
Website: H&H Tube and Manufacturing Co.
Lewis Brass & Copper Company

Supplier Type: Service Center

69-60 79Th St
Middle Village, NY 11379-2933
UNITED STATES
(800) 221-5579
Website: Lewis Brass & Copper Company
Email:
Metals USA Specialty Metals Group

Supplier Type: Service Center

3000 Shermer Rd
Northbrook, IL 60062-7713
UNITED STATES
(800) 999-2497
Morris Metal Service, Inc.

Supplier Type: Service Center

16 Drennan St
Houston, TX 77003-1912
UNITED STATES
(713) 228-9031
(713) 228-2725
Website: Morris Metal Service, Inc.
Olympic Metals, Inc.

Supplier Type: Service Center

5775 Monaco St
Commerce City, CO 80022-4064
UNITED STATES
(303) 286-9700
Website: Olympic Metals, Inc.
Email:
Precision Tube Company, LLC

Supplier Type: Fabricator

287 Wissahickon Ave
North Wales, PA 19454-4115
UNITED STATES
(215) 699-5801
(215) 699-0761
Website: Precision Tube Company, LLC
Email:
Scioto Metals, Inc.

Supplier Type: Service Center

209 Green Meadows Dr S
Lewis Center, OH 43035-9460
UNITED STATES
(614) 885-8213
(614) 885-7382
Website: Scioto Metals, Inc.
Email:
Seeger Metals & Plastics, Inc.

Supplier Type: Service Center

1315 E Manhattan Blvd
Toledo, OH 43608-1523
UNITED STATES
(419) 729-9757
(419) 729-7781
Website: Seeger Metals & Plastics, Inc.
Email:
Sequoia Brass & Copper

Supplier Type: Service Center

2289 Industrial Pkwy W
Hayward, CA 94545-5026
UNITED STATES
(510) 887-5525
(510) 887-0601
Website: Sequoia Brass & Copper
Email:
Small Tube ProductsA member of the CDA

Supplier Type: Fabricator

Contact: Stephen L. Drew
PO BOX 1017
200 Oliphant Dr.
Duncansville, PA 16635-1017
UNITED STATES
(814) 693-6000
(814) 696-0702
Website: Small Tube Products
United States Brass & Copper

Supplier Type: Service Center

1401 Brook Dr
Downers Grove, IL 60515-1077
UNITED STATES
(630) 629-9340
(630) 629-9350
Website: United States Brass & Copper
Email:

C33000 Wire

Please note: Alloys marked with * are registered with the U.S. EPA as Antimicrobial