Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (1) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (0) You Searched For: coated-metal-arc-welding:"Fair" soldering:"Fair" modulus-of-elasticity-in-tension:[14000 TO 15000] CLEAR this search X SAVE this search << Page 1 >> 1 Alloys Found Alloy UNS#DesignationActiveView C86550 Yes C86550 Profile Suppliers of C86550 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>