Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (0) You Searched For: electrical-conductivity:[80.0 TO 85.0] oxyacetylene-welding:"Not Recommended" CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C18020 Yes C18020 Profile Suppliers of C18020 C18100 Yes C18100 Profile Suppliers of C18100 C18147 Yes C18147 Profile Suppliers of C18147 C18148 Yes C18148 Profile Suppliers of C18148 C18200 Chromium Copper Yes C18200 Profile Suppliers of C18200 C18400 Chromium Copper Yes C18400 Profile Suppliers of C18400 C18500 High Copper No C18500 Profile Suppliers of C18500 C81500 Chrome Copper Yes C81500 Profile Suppliers of C81500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>