Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: butt-weld:"Excellent" modulus-of-elasticity-in-tension:[18000 TO 19000] oxyacetylene-welding:"Good" CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C64751 Yes C64751 Profile Suppliers of C64751 C64752 Yes C64752 Profile Suppliers of C64752 C72900 * Yes C72900 Profile Suppliers of C72900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>