Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (2) You Searched For: capacity-for-being-hot-formed:"Excellent" capacity-for-being-cold-worked:"Excellent" element_names:"Cadmium" CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C14300 * Cadmium Copper, Deoxidized Yes C14300 Profile Suppliers of C14300 C14310 * Cadmium Copper No C14310 Profile Suppliers of C14310 C28340 Yes C28340 Profile Suppliers of C28340 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>