Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: butt-weld:"Excellent" rockwell-30t-scale:[45 TO 50] CLEAR this search X SAVE this search << Page 1 >> 2 Alloys Found Alloy UNS#DesignationActiveView C51100 * Yes C51100 Profile Suppliers of C51100 C66700 * Manganese Brass Yes C66700 Profile Suppliers of C66700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>