Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (0) You Searched For: elongation:[51 TO 54] modulus-of-elasticity-in-tension:[13000 TO 14000] rockwell-b-scale:[70 TO 80] yield-strength:[10 TO 30] CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C36000 Free-Cutting Brass Yes C36000 Profile Suppliers of C36000 C36010 Leaded Brass (Free-Cutting Brass) Yes C36010 Profile Suppliers of C36010 C36200 Leaded Brass No C36200 Profile Suppliers of C36200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>