Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: elongation:[57 TO 60] rockwell-b-scale:[70 TO 80] seam-weld:"Fair" CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C68320 Yes C68320 Profile Suppliers of C68320 C85570 Yes C85570 Profile Suppliers of C85570 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>