Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (8) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (6) You Searched For: capacity-for-being-cold-worked:"Excellent" melting-point-solidus:[1950 TO 2000] element_names:"Tin" CLEAR this search X SAVE this search << Page 1 >> 8 Alloys Found Alloy UNS#DesignationActiveView C18060 Yes C18060 Profile Suppliers of C18060 C18620 * Hiigh Copper Yes C18620 Profile Suppliers of C18620 C18625 * HRSC Yes C18625 Profile Suppliers of C18625 C19026 Yes C19026 Profile Suppliers of C19026 C19500 * Yes C19500 Profile Suppliers of C19500 C19720 * Yes C19720 Profile Suppliers of C19720 C64760 * Yes C64760 Profile Suppliers of C64760 C70310 * Yes C70310 Profile Suppliers of C70310 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>