Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (1) You Searched For: coated-metal-arc-welding:"Fair" shrinkage-in-solidification:"Medium" modulus-of-elasticity-in-tension:[15000 TO 16000] CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C81800 * Copper Beryllium 50C No C81800 Profile Suppliers of C81800 C84800 Plumbing Goods Brass Yes C84800 Profile Suppliers of C84800 C87200 Silicon Bronze No C87200 Profile Suppliers of C87200 C90500 Gun Metal Yes C90500 Profile Suppliers of C90500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>