Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (4) You Searched For: density:[0.29 TO 0.3] gas-shielded-arc-welding:"Excellent" electrical-conductivity:[5.0 TO 10.0] CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C63800 * Yes C63800 Profile Suppliers of C63800 C87500 * Coppe Silicon Alloy Yes C87500 Profile Suppliers of C87500 C87600 * Copper Silcon Alloy Yes C87600 Profile Suppliers of C87600 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>