Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (1) You Searched For: density:[0.31 TO 0.32] electrical-conductivity:[15.0 TO 20.0] coated-metal-arc-welding:"Not Recommended" CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C27460 Yes C27460 Profile Suppliers of C27460 C54400 Phosphor Bronze B-2 Yes C54400 Profile Suppliers of C54400 C83450 Yes C83450 Profile Suppliers of C83450 C89842 * Copper-Zinc-Tin-Bismuth Yes C89842 Profile Suppliers of C89842 C89844 Yes C89844 Profile Suppliers of C89844 C93500 Yes C93500 Profile Suppliers of C93500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>