Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (1) U.S. EPA Registered Antimicrobial (6) You Searched For: elongation:[12 TO 15] melting-point-liquidus:[1900 TO 2000] melting-point-solidus:[1750 TO 1800] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C19910 * NKT 322 (High Copper) Yes C19910 Profile Suppliers of C19910 C51000 * Phosphor Bronze, 5% A Yes C51000 Profile Suppliers of C51000 C51100 * Yes C51100 Profile Suppliers of C51100 C51180 * Yes C51180 Profile Suppliers of C51180 C72600 * Copper Nickel No C72600 Profile Suppliers of C72600 C82000 * Copper Beryllium 10C Yes C82000 Profile Suppliers of C82000 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>