Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (2) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: elongation:[27 TO 30] melting-point-liquidus:[1800 TO 1900] tensile-strength:[140 TO 150] CLEAR this search X SAVE this search << Page 1 >> 2 Alloys Found Alloy UNS#DesignationActiveView C52480 * Yes C52480 Profile Suppliers of C52480 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>