Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: butt-weld:"Excellent" melting-point-solidus:[2000 TO *] CLEAR this search X SAVE this search << Page 1 >> 3 Alloys Found Alloy UNS#DesignationActiveView C70600 * Copper-Nickel, 10% Yes C70600 Profile Suppliers of C70600 C71000 * Copper-Nickel, 20% Yes C71000 Profile Suppliers of C71000 C71500 * Copper-Nickel, 30% Yes C71500 Profile Suppliers of C71500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>