Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (15) Inactive Alloys (4) U.S. EPA Registered Antimicrobial (16) You Searched For: capacity-for-being-cold-worked:"Excellent" element_names:"Silver" CLEAR this search X SAVE this search << Page 1 >> 19 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C10400 * Oxygen-Free with Ag (OFS) Yes C10400 Profile Suppliers of C10400 C10500 * Oxygen-Free with Ag (OFS) Yes C10500 Profile Suppliers of C10500 C10700 * Oxygen-Free with Ag (OFS) Yes C10700 Profile Suppliers of C10700 C11300 * Tough Pitch with Ag (STP) Yes C11300 Profile Suppliers of C11300 C11400 * Tough Pitch with Ag (STP) Yes C11400 Profile Suppliers of C11400 C11500 * Tough Pitch with Ag (STP) Yes C11500 Profile Suppliers of C11500 C11600 * Tough Pitch with Ag (STP) Yes C11600 Profile Suppliers of C11600 C12100 * Phosphorus-Deoxidized, Low Residual P (DLPS) Yes C12100 Profile Suppliers of C12100 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C15500 * Yes C15500 Profile Suppliers of C15500 C18080 Yes C18080 Profile Suppliers of C18080 C18500 High Copper No C18500 Profile Suppliers of C18500 C19002 * Yes C19002 Profile Suppliers of C19002 C70310 * Yes C70310 Profile Suppliers of C70310 C70370 * Yes C70370 Profile Suppliers of C70370 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>