7 Alloys Found

Alloy UNS#DesignationActiveView

C27460

Yes C27460 Profile
Suppliers of C27460

C49300 *

Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile
Suppliers of C49300

C49350 *

Bismuth Brass Alloy Yes C49350 Profile
Suppliers of C49350

C67340

Yes C67340 Profile
Suppliers of C67340

C67420

Yes C67420 Profile
Suppliers of C67420

C68800 *

Yes C68800 Profile
Suppliers of C68800

C69000 *

Copper Zinc No C69000 Profile
Suppliers of C69000