Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: density:[0.29 TO 0.3] tensile-strength:[150 TO 160] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C17300 Copper Beryllium Yes C17300 Profile Suppliers of C17300 C82400 * Copper Beryllium 165C Yes C82400 Profile Suppliers of C82400 C82500 * Copper Beryllium 20C Yes C82500 Profile Suppliers of C82500 C82510 * Copper Beryllium 21C Yes C82510 Profile Suppliers of C82510 C82700 * High Copper Alloy Yes C82700 Profile Suppliers of C82700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>