Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (6) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: capacity-for-being-hot-formed:"Excellent" capacity-for-being-cold-worked:"Poor" melting-point-solidus:[1500 TO 1550] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C46750 Yes C46750 Profile Suppliers of C46750 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C49350 * Bismuth Brass Alloy Yes C49350 Profile Suppliers of C49350 C69350 Yes C69350 Profile Suppliers of C69350 C69400 Silicon Red Brass Yes C69400 Profile Suppliers of C69400 C69410 Yes C69410 Profile Suppliers of C69410 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>