Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
13 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C27250 |
Yes |
C27250 Profile Suppliers of C27250 |
|
C27550 |
Yes |
C27550 Profile Suppliers of C27550 |
|
C60600 * |
Aluminum Bronze | No |
C60600 Profile Suppliers of C60600 |
C68370 |
Yes |
C68370 Profile Suppliers of C68370 |
|
C85450 * |
Copper Zinc Alloy | Yes |
C85450 Profile Suppliers of C85450 |
C86550 |
Yes |
C86550 Profile Suppliers of C86550 |
|
C87400 |
Yes |
C87400 Profile Suppliers of C87400 |
|
C87870 * |
Yes |
C87870 Profile Suppliers of C87870 |
|
C87950 |
Yes |
C87950 Profile Suppliers of C87950 |
|
C89545 |
Yes |
C89545 Profile Suppliers of C89545 |
|
C89720 * |
Copper-Bismuth Alloy (TECO) | Yes |
C89720 Profile Suppliers of C89720 |
C99760 * |
Yes |
C99760 Profile Suppliers of C99760 |
|
C99770 * |
Yes |
C99770 Profile Suppliers of C99770 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |