You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C44300 * |
Admiralty, Arsenical | Yes |
C44300 Profile Suppliers of C44300 |
C44400 * |
Admiralty, Antimonial | Yes |
C44400 Profile Suppliers of C44400 |
C44500 * |
Admiralty, Phosphorized | Yes |
C44500 Profile Suppliers of C44500 |
C52100 * |
Phospher Bronze, 8% C | Yes |
C52100 Profile Suppliers of C52100 |
C52180 * |
Yes |
C52180 Profile Suppliers of C52180 |
|
C76800 |
WNS7 | Yes |
C76800 Profile Suppliers of C76800 |
C79860 |
Yes |
C79860 Profile Suppliers of C79860 |
|
C89720 * |
Copper-Bismuth Alloy (TECO) | Yes |
C89720 Profile Suppliers of C89720 |
C90200 |
Yes |
C90200 Profile Suppliers of C90200 |
|
C99700 |
White Manganese Brass | Yes |
C99700 Profile Suppliers of C99700 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |