Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: rockwell-b-scale:[60 TO 70] tensile-strength:[60 TO 70] gas-shielded-arc-welding:"Excellent" CLEAR this search X SAVE this search << Page 1 >> 5 Alloys Found Alloy UNS#DesignationActiveView C19400 * Yes C19400 Profile Suppliers of C19400 C42200 * Yes C42200 Profile Suppliers of C42200 C65500 * High-Silicon Bronze A Yes C65500 Profile Suppliers of C65500 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 C95300 * Yes C95300 Profile Suppliers of C95300 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>