Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (5) Inactive Alloys (2) U.S. EPA Registered Antimicrobial (1) You Searched For: rockwell-b-scale:[70 TO 80] elongation:[45 TO 48] melting-point-solidus:[1600 TO 1650] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C28000 * Muntz Metal, 60% Yes C28000 Profile Suppliers of C28000 C34000 Medium Leaded Brass, 64-1/2% Yes C34000 Profile Suppliers of C34000 C35000 Medium Leaded Brass, 62% Yes C35000 Profile Suppliers of C35000 C46400 Naval Brass, Uninhibited Yes C46400 Profile Suppliers of C46400 C46500 Naval Brass, Arsenical Yes C46500 Profile Suppliers of C46500 C46600 Tin Brass No C46600 Profile Suppliers of C46600 C46700 Tin Brass No C46700 Profile Suppliers of C46700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>