Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (7) You Searched For: rockwell-b-scale:[70 TO 80] electrical-conductivity:[40.0 TO 45.0] CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C17500 * Copper Beryllium Yes C17500 Profile Suppliers of C17500 C17510 * Copper Beryllium Yes C17510 Profile Suppliers of C17510 C22000 * Commercial Bronze, 90% Yes C22000 Profile Suppliers of C22000 C22600 * Jewelry Bronze, 87-1/2% Yes C22600 Profile Suppliers of C22600 C40500 * Penny Bronze Yes C40500 Profile Suppliers of C40500 C82000 * Copper Beryllium 10C Yes C82000 Profile Suppliers of C82000 C82200 * Copper Beryllium 3C Yes C82200 Profile Suppliers of C82200 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>