Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (3) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (1) You Searched For: butt-weld:"Fair" capacity-for-being-hot-formed:"Excellent" elongation:[45 TO 48] CLEAR this search X SAVE this search << Page 1 >> 6 Alloys Found Alloy UNS#DesignationActiveView C17200 * Copper Beryllium Yes C17200 Profile Suppliers of C17200 C36500 Leaded Muntz Metal, Uninhibited Yes C36500 Profile Suppliers of C36500 C36600 Leaded Muntz Metal, Arsinical No C36600 Profile Suppliers of C36600 C36700 Leaded Muntz Metal, Antimonial No C36700 Profile Suppliers of C36700 C36800 Leaded Brass No C36800 Profile Suppliers of C36800 C37700 Forging Brass Yes C37700 Profile Suppliers of C37700 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>