11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C17200
*
|
Copper Beryllium | Yes |
C17200 Profile Suppliers of C17200 |
C17300
|
Copper Beryllium | Yes |
C17300 Profile Suppliers of C17300 |
C63800
*
|
Yes |
C63800 Profile Suppliers of C63800 |
|
C66900
*
|
Manganese Brass | Yes |
C66900 Profile Suppliers of C66900 |
C68800
*
|
Yes |
C68800 Profile Suppliers of C68800 |
|
C69000
*
|
Copper Zinc | No |
C69000 Profile Suppliers of C69000 |
C69300
*
|
ECO Brass | Yes |
C69300 Profile Suppliers of C69300 |
C69400
|
Silicon Red Brass | Yes |
C69400 Profile Suppliers of C69400 |
C69410
|
Yes |
C69410 Profile Suppliers of C69410 |
|
C69710
|
Yes |
C69710 Profile Suppliers of C69710 |
|
C87800
*
|
Cast Silicon Bronze | Yes |
C87800 Profile Suppliers of C87800 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |