Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (4) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: electrical-conductivity:[30.0 TO 35.0] melting-point-liquidus:[1800 TO 1900] rockwell-b-scale:[70 TO 80] CLEAR this search X SAVE this search << Page 1 >> 4 Alloys Found Alloy UNS#DesignationActiveView C24000 * Low Brass, 80% Yes C24000 Profile Suppliers of C24000 C31600 Leaded Commercial Bronze (Nickel-Bearing) Yes C31600 Profile Suppliers of C31600 C41300 * Tin Brass Yes C41300 Profile Suppliers of C41300 C43400 * Yes C43400 Profile Suppliers of C43400 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>