Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (23) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (14) You Searched For: density:[0.29 TO 0.3] density:[0.3 TO 0.31] element_names:"Silicon" CLEAR this search X SAVE this search << Page 1 >> 23 Alloys Found Alloy UNS#DesignationActiveView C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C49355 * Copper Zinc Bismuth Alloy Yes C49355 Profile Suppliers of C49355 C67300 Yes C67300 Profile Suppliers of C67300 C68330 Yes C68330 Profile Suppliers of C68330 C68370 Yes C68370 Profile Suppliers of C68370 C69220 * Copper Zinc Alloy Yes C69220 Profile Suppliers of C69220 C69300 * ECO Brass Yes C69300 Profile Suppliers of C69300 C69305 Yes C69305 Profile Suppliers of C69305 C69310 * SnEco Yes C69310 Profile Suppliers of C69310 C69710 Yes C69710 Profile Suppliers of C69710 C79860 Yes C79860 Profile Suppliers of C79860 C86550 Yes C86550 Profile Suppliers of C86550 C87400 Yes C87400 Profile Suppliers of C87400 C87600 * Copper Silcon Alloy Yes C87600 Profile Suppliers of C87600 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 C87845 * Copper-Silicon-Brass Yes C87845 Profile Suppliers of C87845 C87850 * Copper Silicon Alloy Yes C87850 Profile Suppliers of C87850 C87860 * Yes C87860 Profile Suppliers of C87860 C87870 * Yes C87870 Profile Suppliers of C87870 C87950 Yes C87950 Profile Suppliers of C87950 C89720 * Copper-Bismuth Alloy (TECO) Yes C89720 Profile Suppliers of C89720 C99400 * Non-Dezincificztion Alloy Yes C99400 Profile Suppliers of C99400 C99500 * Special Alloys Yes C99500 Profile Suppliers of C99500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>