Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (3) U.S. EPA Registered Antimicrobial (11) You Searched For: element_names:"Antimony" element_names:"Lead" elongation:[6 TO 9] CLEAR this search X SAVE this search << Page 1 >> 22 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12510 * Yes C12510 Profile Suppliers of C12510 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C49300 * Lead-Free Bismuth Alloy (Lead-Free) Yes C49300 Profile Suppliers of C49300 C72800 * Yes C72800 Profile Suppliers of C72800 C87850 * Copper Silicon Alloy Yes C87850 Profile Suppliers of C87850 C89550 * SeBiLOY III (EnviroBrass III) Yes C89550 Profile Suppliers of C89550 C92700 Leaded Tin Bronze Yes C92700 Profile Suppliers of C92700 C92900 Yes C92900 Profile Suppliers of C92900 C93400 Yes C93400 Profile Suppliers of C93400 C93700 Bearing Bronze Yes C93700 Profile Suppliers of C93700 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 C94100 Yes C94100 Profile Suppliers of C94100 C94300 Soft Bronze Yes C94300 Profile Suppliers of C94300 C94800 Yes C94800 Profile Suppliers of C94800 C97300 Yes C97300 Profile Suppliers of C97300 C97800 Yes C97800 Profile Suppliers of C97800 C99760 * Yes C99760 Profile Suppliers of C99760 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>