Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (7) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (5) You Searched For: elongation:[21 TO 24] coated-metal-arc-welding:"Good" CLEAR this search X SAVE this search << Page 1 >> 7 Alloys Found Alloy UNS#DesignationActiveView C61800 * Yes C61800 Profile Suppliers of C61800 C61900 * Yes C61900 Profile Suppliers of C61900 C62300 * Aluminum Bronze, 9% Yes C62300 Profile Suppliers of C62300 C63200 * Aluminum Bronze Yes C63200 Profile Suppliers of C63200 C69240 Yes C69240 Profile Suppliers of C69240 C69410 Yes C69410 Profile Suppliers of C69410 C70400 * Copper-Nickel, 5% Yes C70400 Profile Suppliers of C70400 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>