Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C23000 * |
Red Brass, 85% | Yes |
C23000 Profile Suppliers of C23000 |
C24000 * |
Low Brass, 80% | Yes |
C24000 Profile Suppliers of C24000 |
C26000 * |
Cartridge Brass, 70% | Yes |
C26000 Profile Suppliers of C26000 |
C33500 |
Low-Leaded Brass | Yes |
C33500 Profile Suppliers of C33500 |
C41100 * |
Tin Brass | Yes |
C41100 Profile Suppliers of C41100 |
C41300 * |
Tin Brass | Yes |
C41300 Profile Suppliers of C41300 |
C41500 * |
Tin Brass | Yes |
C41500 Profile Suppliers of C41500 |
C43000 * |
Tin Brass | Yes |
C43000 Profile Suppliers of C43000 |
C64400 * |
Aluminum Bronze | No |
C64400 Profile Suppliers of C64400 |
C66430 * |
Yes |
C66430 Profile Suppliers of C66430 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |