Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C15100 * |
Yes |
C15100 Profile Suppliers of C15100 |
|
C17200 * |
Copper Beryllium | Yes |
C17200 Profile Suppliers of C17200 |
C19400 * |
Yes |
C19400 Profile Suppliers of C19400 |
|
C28000 * |
Muntz Metal, 60% | Yes |
C28000 Profile Suppliers of C28000 |
C37000 |
Free-Cutting Muntz Metal | Yes |
C37000 Profile Suppliers of C37000 |
C37100 |
Yes |
C37100 Profile Suppliers of C37100 |
|
C46400 |
Naval Brass, Uninhibited | Yes |
C46400 Profile Suppliers of C46400 |
C46500 |
Naval Brass, Arsenical | Yes |
C46500 Profile Suppliers of C46500 |
C65100 * |
Low-Silicon Bronze B | Yes |
C65100 Profile Suppliers of C65100 |
C65500 * |
High-Silicon Bronze A | Yes |
C65500 Profile Suppliers of C65500 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |