Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
11 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C51080 * |
Yes |
C51080 Profile Suppliers of C51080 |
|
C61000 * |
Yes |
C61000 Profile Suppliers of C61000 |
|
C64400 * |
Aluminum Bronze | No |
C64400 Profile Suppliers of C64400 |
C83450 |
Yes |
C83450 Profile Suppliers of C83450 |
|
C83600 |
Ounce Metal | Yes |
C83600 Profile Suppliers of C83600 |
C84010 * |
Semi-Red Brass | Yes |
C84010 Profile Suppliers of C84010 |
C84020 * |
Semi-Red Brass | Yes |
C84020 Profile Suppliers of C84020 |
C85450 * |
Copper Zinc Alloy | Yes |
C85450 Profile Suppliers of C85450 |
C89836 |
Copper Bismuth Alloy | Yes |
C89836 Profile Suppliers of C89836 |
C89837 |
Yes |
C89837 Profile Suppliers of C89837 |
|
C89844 |
Yes |
C89844 Profile Suppliers of C89844 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |