Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (17) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (3) You Searched For: density:[0.31 TO 0.32] melting-point-solidus:[1550 TO 1600] soldering:"Excellent" CLEAR this search X SAVE this search << Page 1 >> 17 Alloys Found Alloy UNS#DesignationActiveView C52400 * Phospher Bronze 10% D Yes C52400 Profile Suppliers of C52400 C52480 * Yes C52480 Profile Suppliers of C52480 C69750 Yes C69750 Profile Suppliers of C69750 C83450 Yes C83450 Profile Suppliers of C83450 C83600 Ounce Metal Yes C83600 Profile Suppliers of C83600 C83800 Hydraulic Bronze Yes C83800 Profile Suppliers of C83800 C89836 Copper Bismuth Alloy Yes C89836 Profile Suppliers of C89836 C89842 * Copper-Zinc-Tin-Bismuth Yes C89842 Profile Suppliers of C89842 C89844 Yes C89844 Profile Suppliers of C89844 C90300 Tin Bronze Yes C90300 Profile Suppliers of C90300 C90500 Gun Metal Yes C90500 Profile Suppliers of C90500 C91600 Yes C91600 Profile Suppliers of C91600 C91700 Nickel Gear Bronze Yes C91700 Profile Suppliers of C91700 C92300 Leaded Tin Bronze Yes C92300 Profile Suppliers of C92300 C92600 Yes C92600 Profile Suppliers of C92600 C92700 Leaded Tin Bronze Yes C92700 Profile Suppliers of C92700 C92900 Yes C92900 Profile Suppliers of C92900 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>