28 Alloys Found

Alloy UNS#DesignationActiveView

C18835 *

Yes C18835 Profile
Suppliers of C18835

C19002 *

Yes C19002 Profile
Suppliers of C19002

C19010 *

Yes C19010 Profile
Suppliers of C19010

C19500 *

Yes C19500 Profile
Suppliers of C19500

C49355 *

Copper Zinc Bismuth Alloy Yes C49355 Profile
Suppliers of C49355

C61900 *

Yes C61900 Profile
Suppliers of C61900

C62400 *

Aluminum Bronze,11% Yes C62400 Profile
Suppliers of C62400

C65100 *

Low-Silicon Bronze B Yes C65100 Profile
Suppliers of C65100

C67400

Yes C67400 Profile
Suppliers of C67400

C67420

Yes C67420 Profile
Suppliers of C67420

C68800 *

Yes C68800 Profile
Suppliers of C68800

C69000 *

Copper Zinc No C69000 Profile
Suppliers of C69000

C69230 *

Yes C69230 Profile
Suppliers of C69230

C69240

Yes C69240 Profile
Suppliers of C69240

C69300 *

ECO Brass Yes C69300 Profile
Suppliers of C69300

C69310 *

SnEco Yes C69310 Profile
Suppliers of C69310

C69350

Yes C69350 Profile
Suppliers of C69350

C69400

Silicon Red Brass Yes C69400 Profile
Suppliers of C69400

C69410

Yes C69410 Profile
Suppliers of C69410

C69430

Yes C69430 Profile
Suppliers of C69430

C69850

Yes C69850 Profile
Suppliers of C69850

C70260 *

Yes C70260 Profile
Suppliers of C70260

C70310 *

Yes C70310 Profile
Suppliers of C70310

C72500 *

Yes C72500 Profile
Suppliers of C72500

C87850 *

Copper Silicon Alloy Yes C87850 Profile
Suppliers of C87850

C87860 *

Yes C87860 Profile
Suppliers of C87860

C87870 *

Yes C87870 Profile
Suppliers of C87870

C89841

Copper-Bismuth Alloy Yes C89841 Profile
Suppliers of C89841
* signifies an alloy registered with the U.S. EPA as Antimicrobial.