Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (9) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (2) You Searched For: brazing:"Poor" CLEAR this search X SAVE this search << Page 1 >> 9 Alloys Found Alloy UNS#DesignationActiveView C49360 * Tin-Eco(bismuth) Yes C49360 Profile Suppliers of C49360 C86100 Manganese Bronze Yes C86100 Profile Suppliers of C86100 C86200 Yes C86200 Profile Suppliers of C86200 C86300 Manganese Bronze Yes C86300 Profile Suppliers of C86300 C89580 * Yes C89580 Profile Suppliers of C89580 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C93900 79-6-15 Yes C93900 Profile Suppliers of C93900 C94300 Soft Bronze Yes C94300 Profile Suppliers of C94300 C94500 Yes C94500 Profile Suppliers of C94500 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>