10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C24000 * |
Low Brass, 80% | Yes |
C24000 Profile Suppliers of C24000 |
C26000 * |
Cartridge Brass, 70% | Yes |
C26000 Profile Suppliers of C26000 |
C26100 * |
Brass | No |
C26100 Profile Suppliers of C26100 |
C26130 * |
Yes |
C26130 Profile Suppliers of C26130 |
|
C26200 * |
Yes |
C26200 Profile Suppliers of C26200 |
|
C26800 * |
Yellow Brass, 66% | Yes |
C26800 Profile Suppliers of C26800 |
C27000 * |
Yellow Brass, 65% | Yes |
C27000 Profile Suppliers of C27000 |
C52480 * |
Yes |
C52480 Profile Suppliers of C52480 |
|
C61500 * |
Yes |
C61500 Profile Suppliers of C61500 |
|
C65500 * |
High-Silicon Bronze A | Yes |
C65500 Profile Suppliers of C65500 |
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |