Saved Copper Alloys
Saved Searches
Copper Alloy Advanced Search Help
We'd Love Your Input
Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input.
You Searched For:
10 Alloys Found
Alloy UNS# | Designation | Active | View |
---|---|---|---|
C70600 * |
Copper-Nickel, 10% | Yes |
C70600 Profile Suppliers of C70600 |
C71000 * |
Copper-Nickel, 20% | Yes |
C71000 Profile Suppliers of C71000 |
C71500 * |
Copper-Nickel, 30% | Yes |
C71500 Profile Suppliers of C71500 |
C85450 * |
Copper Zinc Alloy | Yes |
C85450 Profile Suppliers of C85450 |
C96200 * |
Yes |
C96200 Profile Suppliers of C96200 |
|
C96300 * |
Yes |
C96300 Profile Suppliers of C96300 |
|
C96400 * |
70-30 Copper Nickel | Yes |
C96400 Profile Suppliers of C96400 |
C96600 * |
Yes |
C96600 Profile Suppliers of C96600 |
|
C97600 |
Yes |
C97600 Profile Suppliers of C97600 |
|
C97800 |
Yes |
C97800 Profile Suppliers of C97800 |
|
* signifies an alloy registered with the U.S. EPA as Antimicrobial. |