Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (19) Inactive Alloys (0) U.S. EPA Registered Antimicrobial (9) You Searched For: casting-yield:"High" elongation:[12 TO 15] CLEAR this search X SAVE this search << Page 1 >> 19 Alloys Found Alloy UNS#DesignationActiveView C82400 * Copper Beryllium 165C Yes C82400 Profile Suppliers of C82400 C82500 * Copper Beryllium 20C Yes C82500 Profile Suppliers of C82500 C82600 * Copper Beryllium 245C Yes C82600 Profile Suppliers of C82600 C83600 Ounce Metal Yes C83600 Profile Suppliers of C83600 C84100 Yes C84100 Profile Suppliers of C84100 C84200 Yes C84200 Profile Suppliers of C84200 C85800 Yes C85800 Profile Suppliers of C85800 C87800 * Cast Silicon Bronze Yes C87800 Profile Suppliers of C87800 C89320 * Yes C89320 Profile Suppliers of C89320 C89510 * SeBiLOY I (EnviroBrass I) Yes C89510 Profile Suppliers of C89510 C89838 Yes C89838 Profile Suppliers of C89838 C89845 * Copper-Bismuth-Alloy Yes C89845 Profile Suppliers of C89845 C93200 Yes C93200 Profile Suppliers of C93200 C93600 Yes C93600 Profile Suppliers of C93600 C93800 Anti-acid Metal Yes C93800 Profile Suppliers of C93800 C94300 Soft Bronze Yes C94300 Profile Suppliers of C94300 C94500 Yes C94500 Profile Suppliers of C94500 C96600 * Yes C96600 Profile Suppliers of C96600 C99760 * Yes C99760 Profile Suppliers of C99760 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>