Saved Copper Alloys Alloy was saved successfully. Saved Searches search criteria was saved successfully. Copper Alloy Advanced Search Help We'd Love Your Input Please give us your feedback on this new Advanced Search of the Copper Alloys database by completing a brief survey. We value your input. Narrow By: Active Alloys (18) Inactive Alloys (5) U.S. EPA Registered Antimicrobial (17) You Searched For: element_names:"Tellurium" CLEAR this search X SAVE this search << Page 1 >> 23 Alloys Found Alloy UNS#DesignationActiveView C10100 * Oxygen-Free-Electronic (OFE) Yes C10100 Profile Suppliers of C10100 C11025 * Fire Refined High Conductivity (FRHC) Yes C11025 Profile Suppliers of C11025 C11040 * Yes C11040 Profile Suppliers of C11040 C11045 * ETP (ETP) Yes C11045 Profile Suppliers of C11045 C11050 ETP-R Yes C11050 Profile Suppliers of C11050 C12500 * Fire-Refined Tough Pitch (FRTP) Yes C12500 Profile Suppliers of C12500 C12510 * Yes C12510 Profile Suppliers of C12510 C12700 * Copper Alloy No C12700 Profile Suppliers of C12700 C12800 * Copper Alloy No C12800 Profile Suppliers of C12800 C12900 * Fire-Refined Tough Pitch with Ag (FRSTP) Yes C12900 Profile Suppliers of C12900 C13000 Copper Alloy No C13000 Profile Suppliers of C13000 C14400 * Copper Alloy No C14400 Profile Suppliers of C14400 C14420 * Yes C14420 Profile Suppliers of C14420 C14500 * Tellurium-Bearing (PTE) Yes C14500 Profile Suppliers of C14500 C14510 * Tellurium-Bearing Yes C14510 Profile Suppliers of C14510 C14520 * Phosphorus-Deoxidized,Tellurium-Bearing (DPTE) Yes C14520 Profile Suppliers of C14520 C14530 * Yes C14530 Profile Suppliers of C14530 C17700 * Copper Beryllium No C17700 Profile Suppliers of C17700 C18050 Yes C18050 Profile Suppliers of C18050 C19100 Yes C19100 Profile Suppliers of C19100 C42210 * Tin Brass Yes C42210 Profile Suppliers of C42210 C49100 Yes C49100 Profile Suppliers of C49100 C72670 Yes C72670 Profile Suppliers of C72670 * signifies an alloy registered with the U.S. EPA as Antimicrobial. << Page 1 >>