36 Alloys Found

Alloy UNS#DesignationActiveView

C15000 *

Zirconium Copper Yes C15000 Profile
Suppliers of C15000

C17000 *

Beryllium Copper Yes C17000 Profile
Suppliers of C17000

C17300

Beryllium Copper Yes C17300 Profile
Suppliers of C17300

C17400 *

Beryllium Copper No C17400 Profile
Suppliers of C17400

C17410 *

Beryllium Copper Yes C17410 Profile
Suppliers of C17410

C17500 *

Beryllium Copper Yes C17500 Profile
Suppliers of C17500

C17530 *

Beryllium Copper Yes C17530 Profile
Suppliers of C17530

C18100

Yes C18100 Profile
Suppliers of C18100

C18600

Yes C18600 Profile
Suppliers of C18600

C18610

Yes C18610 Profile
Suppliers of C18610

C18661 *

Yes C18661 Profile
Suppliers of C18661

C19000 *

Yes C19000 Profile
Suppliers of C19000

C19002 *

Yes C19002 Profile
Suppliers of C19002

C19026

Yes C19026 Profile
Suppliers of C19026

C19210 *

Yes C19210 Profile
Suppliers of C19210

C19217

Yes C19217 Profile
Suppliers of C19217

C40500 *

Penny Bronze Yes C40500 Profile
Suppliers of C40500

C40800 *

Silicon Brass No C40800 Profile
Suppliers of C40800

C41100 *

Tin Brass Yes C41100 Profile
Suppliers of C41100

C41500 *

Tin Brass Yes C41500 Profile
Suppliers of C41500

C42200 *

Yes C42200 Profile
Suppliers of C42200

C42210 *

Tin Brass Yes C42210 Profile
Suppliers of C42210

C43400 *

Yes C43400 Profile
Suppliers of C43400

C64751

Yes C64751 Profile
Suppliers of C64751

C64752

Yes C64752 Profile
Suppliers of C64752

C70280 *

Yes C70280 Profile
Suppliers of C70280

C70290 *

Yes C70290 Profile
Suppliers of C70290

C70310 *

Yes C70310 Profile
Suppliers of C70310

C70370 *

Yes C70370 Profile
Suppliers of C70370

C72800 *

Yes C72800 Profile
Suppliers of C72800

C72900 *

Yes C72900 Profile
Suppliers of C72900

C73500 *

Nickel Silver Yes C73500 Profile
Suppliers of C73500

C75200 *

Nickel Silver, 65-18 Yes C75200 Profile
Suppliers of C75200

C75400

Nickel Silver, 65-15 Yes C75400 Profile
Suppliers of C75400

C75700 *

Nickel Silver, 65-12 Yes C75700 Profile
Suppliers of C75700

C76200

Nickel Silver Yes C76200 Profile
Suppliers of C76200
* signifies an alloy registered with the U.S. EPA as Antimicrobial.